Attentions For Electric Soldering Iron When Making Smart Glass Film Busbar

Attentions For Electric Soldering Iron When Making Smart Glass Film Busbar
By Peter Shin Lin

Attention One:
Before using Electric Soldering Iron, please check if the voltage is suitable.

Attention Two:
If it’s first time the Electric Soldering Iron is used, some smoke
appearing is normal, and the smoke will disappear soon. But please
make sure the working room is good at air ventilation.

Attention Three:
The heating device is made of ceramics, so it’s not very good at
impact resistance, please use with care.

Attention Four:
Please don’t change the devices of the Electric Soldering Iron unless
you are professional. And don’t change devices when the power is on.

Attention Five:
If you need the file of “HOW TO MAKE BUSBAR OF SMART GLASS FILM”,
Please feel free to contact us.

All rights reserved by CNC-INTERLAYER TECH:
【1】CNC-Force® EVA INERLAYER FOR ARCHITECTURAL LAMINATED GLASS
【2】CNC-Smart® SMART FILM FOR PRIVACY SWITCHABLE GLASS
【3】CNC-Shield® PVB INTERLAYER FOR AUTOMOTIVE WINDSHIELD GLASS
Mail: cnc@cncnext.com
Web: www.CNCnext.com
benext77@gmail.com/
benext77@hotmail.com

END.
UPDATED ON 2 MAY 2012

Attentions For Electric Soldering Iron When Making Smart Glass Film Busbar.pdf Download this file

Diy_busbar_of_smart_glass_film

Bubbles in Middle of Safety Laminated Glass of CNC-Shield(R) Polyvinyl Butyral PVB

Bubbles in Middle of Safety Laminated Glass of CNC-Shield® Polyvinyl Butyral PVB

CNC-Shield® Polyvinyl Butyral PVB
Reason Possibility 1:
In the procedure of roller exhausting air, it’s too early to seal the
edges of the pre-laminated glass, so the air can not be exhausted out
completely in the second roller.

Solution:
Adjust the speed and temperature in the pre-laminating procedure, make
sure the pre-laminated glass is not sealed before the second roller
exhausting air stage. Or adjust the speed of and temperature of the
silicone rubber ring, to make sure the air is totally exhausted out.
Reason Possibility 2:
The Polyvinyl Butyral PVB interlayer film already absorbed too much moisture.

Solution:
Check the moisture of the Polyvinyl Butyral PVB interlayer film, and
the humidity of the laminating room and glass surface.

Reason Possibility3:
The plainness of the tempered glass is not good enough.
Solution:
Choose good quality tempered glass, or use thicker Polyvinyl Butyral
PVB interlayer film.

Cnc-shield_polyvinyl_butyral_p

bubbles-in-middle-of-safety-laminated-glass-of-cnc-shield-polyvi.pdf Download this file

Bubbles in Middle of Safety Laminated Glass of CNC-Shield(R) Polyvinyl Butyral PVB

Bubbles in Middle of Safety Laminated Glass of CNC-Shield® Polyvinyl Butyral PVB

CNC-Shield® Polyvinyl Butyral PVB
Reason Possibility 1:
In the procedure of roller exhausting air, it’s too early to seal the
edges of the pre-laminated glass, so the air can not be exhausted out
completely in the second roller.

Solution:
Adjust the speed and temperature in the pre-laminating procedure, make
sure the pre-laminated glass is not sealed before the second roller
exhausting air stage. Or adjust the speed of and temperature of the
silicone rubber ring, to make sure the air is totally exhausted out.
Reason Possibility 2:
The Polyvinyl Butyral PVB interlayer film already absorbed too much moisture.

Solution:
Check the moisture of the Polyvinyl Butyral PVB interlayer film, and
the humidity of the laminating room and glass surface.

Reason Possibility3:
The plainness of the tempered glass is not good enough.
Solution:
Choose good quality tempered glass, or use thicker Polyvinyl Butyral
PVB interlayer film.

bubbles-in-middle-of-safety-laminated-glass-of-cnc-shield-polyvi.pdf Download this file

Cnc-shield_polyvinyl_butyral_p

Bubbles at Edges of Laminated Glass with Polyvinyl Butyral PVB interlayer film

Bubbles at Edges of Laminated Glass with Polyvinyl Butyral PVB interlayer film
PETER SHIN LIN
www.helloglass.com

Condition:
Small bubbles at the edges of safety laminated glass with Polyvinyl
Butyral PVB interlayer film.

Reason: 1)
When the autoclave decreasing the pressure, although the temperature
detector shows the temperature is under 50 degree Celsius, due to the
glass thickness and square, sometimes, the glass temperature is still
higher than 50 degree Celsius, so if the pressure is lowering, some
air will absorbed into the glass edges.

Solution:
Even when the temperature detector shows the temperature is lower than
 50 degree, don’t decrease the pressure too hurry, wait for some
minutes, make sure the real temperature of the glass is lower than 50
degree. If the laminated glass is thick, or many layers, or large
square, then the waiting time should be a little longer.

Reason:2)
The tempered glass is not high quality enough, and the plainness of
the tempered glass is not good enough.

Solution:
Choose better quality tempered glass, or use the thicker Polyvinyl
Butyral PVB interlayer film.

Reason:3)
Maybe the detector of the temperature and pressure is not correct.

Solution:
Make sure the temperature and pressure parameters is correct .

ALL RIGHT RESERVED BY CNC-INTERLAYER TECH:
【1】CNC-Force® EVA INERLAYER FOR ARCHITECTURAL LAMINATED GLASS
【2】CNC-Smart® SMART FILM FOR PRIVACY SWITCHABLE GLASS
【3】CNC-Shield® PVB INTERLAYER FOR AUTOMOTIVE WINDSHIELD GLASS
Mail: cnc@cncnext.com
Web: www.CNCnext.com
benext77@gmail.com/
benext77@hotmail.com

Bubbles at Edges of Laminated Glass with Polyvinyl Butyral PVB interlayer film .pdf Download this file

Bubbles_laminated_glass_pvb_fi

Product Name:Heat fusing furnace

Product_nameheat_fusing_furnac

GLASS MANUFACTURER MAIN PRODUCT
======================================
Product Name:Heat fusing furnace
Product Description:
This equipment can produce circle or single furnace fused frame
glass,screen,glass tableware etc.It can also use in decorating glass
processing(it can be add another one or two cooling cabinet if produce
circularly).Operating by PLC, heating up automatically in whole
processing.the furnace lid rises up and down by electricity.Low
electricity consumption,heating evenly,high efficiency .

Main Technique Parameters
1.outside size:1950*1380*1270mm depend on customer requirements
2.Inner size:1570*1070*200mm
3.Processing thickness:3-25mm
4.rate of work :24KW
5.Total weight:1.8T

======================================
GLASS MANUFACTURER PRODUCT LIST
======================================

Products
Heating equipment
Deep procossing
Glass consumables

======================================
GLASS MANUFACTURER CONTACT INFO
======================================

Name:Foshan Jiachen Machinery Co., LTD
Contact:Mr.Xie
Tel:86-757-88776368
Mob:137 2634 7800
Fax:86-757-88776368
E-mail:fsjiachen@yahoo.cn
Post Code:528226
Address:No.8 ,the Jiebian 7stars Industrial B Zone,No.8,LuoCun
District,Foshan City,Guangdong P.R.China

======================================
GLASS MANUFACTURER COMPANY PROFILE
======================================
Foshan Two-Win Glass Machinery Co., LTD -We are professional in
research and development, production and process. We are located in
the economically developed and beautiful environment and we are in the
China’s Glass Machinery Center – Foshan City.
Our main glass products include glass heat processing machines, glass
deep processing machines and glass consumable items.
We have been persisting in our principle of “Customer First, Forging
Ahead”. We have won a good reputation among customers with good
quality, competitive prices and advanced techniques since our
establishment.
If you are interested in any of our products or would like to discuss
a custom order, please feel free to contact us. We are looking forward
to forming successful business relationships with new clients around
the world in the near future.